Polymer Property : Heat of Vaporization = 90800 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Vaporization 90800 J/g

@Temperature 190 °C
39100 BTU/lb

@Temperature 374 °F
Dow Corning 702 DIFFUSION PUMP FLUID
A clear, mixed phenylmethyl dimethyl cyclosiloxane fluid designed for fast pumping of large volumes of gas down from 10-5 to 10-7. Also used on vapor ejector pumps that attain vacuums of 10-4 to 10-..