Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 201.0 J/g | 86.45 BTU/lb | |
3M Novec™ 71DE Engineered Fluid 3M™ Novec™ 71DE is an azeotrope containing 3M™ Novec™ 7100 and 1,2 trans-dichloroethylene. It maintains a constant liquid and vapor composition at its boiling point. It can be used in many mediu.. |