Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 6490 J/g | 2790 BTU/lb | Latent |
ATI Wah Chang Zircadyne® Alloy Zr 702 Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A.. |