Thermal Properties Metric English Comments
Heat of Vaporization 146 J/g
62.8 BTU/lb
b.p.
Asahi Glass ASAHIKLIN AK-225FPL Hydrochlorofluorocarbon Solvent
AK-225FPL is a mixture of HCFC-225 and a fluorinated solvent. This blend was developed for those customers needing a solvent which is compatible with common plastics, such as polymethylmethacrylate,..