Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 105 J/g | 45.2 BTU/lb | Latent, at normal boiling point |
3M Fluorinert™ FC-3284 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package test.. |