Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 70.0 J/g | 30.1 BTU/lb | Latent, at normal boiling point |
3M Fluorinert™ FC-43 Electronic Liquid 3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct.. |