Polymer Property : Heat of Vaporization = 29.7 BTU/lb Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Vaporization 69.0 J/g
29.7 BTU/lb
Latent, at normal boiling point
3M Fluorinert™ FC-40 Electronic Liquid
3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind..
Heat of Vaporization 69.0 J/g
29.7 BTU/lb
Latent, at normal boiling point
3M Fluorinert™ FC-70 Electronic Liquid
Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a..