Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 179.4 J/g | 77.18 BTU/lb | calculated |
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong.. |