Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 344 J/g | 148 BTU/lb | |
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |