Polymer Property : Heat of Vaporization = 125.6 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Vaporization 125.6 J/g
54.03 BTU/lb
3M Novec™ 71IPA Engineered Fluid
3M™ Novec™ 71IPA Engineered Fluid is ideal for light cleaning and degreasing tasks. 3M™ Novec™ 71IPA has essentially constant vapor and liquid composition at its boiling point. Excellent replace..
Heat of Vaporization 125.6 J/g
54.03 BTU/lb
3M Novec™ 7200 Engineered Fluid
3M™ Novec™ 7200 fluid's convenient boiling point and excellent environmental, health and safety profile make it useful as a heat transfer fluid, cleaning solvent, for lubricant deposition & many m..
Heat of Vaporization 125.6 J/g
54.03 BTU/lb
@ boiling point
3M Novec™ 8200 Engineered Fluid
3M™ Novec™ 8200 Engineered Fluid is a clear, colorless, low-odor fluid intended to replace 1,1,1-trichloroethane and perchloroethylene in film cleaning applications.Features and Benefits:Zero ozon..