Thermal Properties Metric English Comments
Heat Distortion Temperature 78.9 - 94.0 °C
174 - 201 °F
Average value: 84.2 °C Grade Count:6
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..