Polymer Property : Heat Distortion Temperature = 57.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 57.2 °C
135 °F
ASTM D648
BCC Products Proto-Kast BC 8163 Urethane Casting
BC 8163 is a very low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8163 is non-sensitive to moisture after cure and..