Heat Distortion Temperature 248 °C
478 °F
ISO 75-2
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..