Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | >= 237 °C | >= 459 °F | ASTM D648 |
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Heat Distortion Temperature | >= 237 °C | >= 459 °F | ASTM D648 |
Ensinger Tecapeek® XP-98 Medical Compression Molded PEEK Compound, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |