Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 160 °C | 320 °F | ISO 75-2 |
Tisan TISESTER® UNR Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Heat Distortion Temperature | 160 °C | 320 °F | ISO 75-2 |
Tisan TISOPLEN® 30% Glass Fiber Filled Reinforced Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |