Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 115 °C | 239 °F | ISO 75/B |
Iran Petrochemical (PCC) X 30 G Polypropylene X30G is for injection molding because of its good flow properties this grade offers easy processing and extruded items exhibit high stiffness.Applications: The grade is widely used for injection mol.. |
|||
Heat Distortion Temperature | 115 °C | 239 °F | ISO 75/B |
Iran Petrochemical (PCC) X 30 S Polypropylene Film Polypropylene film with good optical propertiesApplications: film, packing food stuffs, stationary and textiles.Information provided by Iran Petrochemical Commercial Co. |