Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | >= 235 °C | >= 455 °F | ASTM D648 |
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |