Polymer Property : Heat Distortion Temperature = 214 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 214 °C
417 °F
ISO 75-2
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..