Polymer Property : Heat Distortion Temperature = 200 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 200 °C
392 °F
ISO 75 A/B
Tisan TISAPET® UNR Polyethylene Terephthalate
Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a..
Heat Distortion Temperature 200 °C
392 °F
ISO 75-2
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Heat Distortion Temperature 200 °C
392 °F
ISO 75-2
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..