Thermal Properties Metric English Comments
Heat Distortion Temperature 70.0 °C
158 °F
Lord Adhesives Circalokâ„¢ 6031 A/B Epoxy Encapsulant
Circalokâ„¢ 6031 A/B is a two-part epoxy potting compound with excellent electrical properties at elevated temperatures. Good arc-track resistance under high voltage loading and other dielectric ..
Heat Distortion Temperature >= 70.0 °C
>= 158 °F
ASTM D 648
Karina 822-18/599-CRB-LMP Gray PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 70.0 °C
>= 158 °F
ASTM D 648
Karina E 822-10/148-CRB-LMP White PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.