Polymer Property : Heat Distortion Temperature = 143 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 143 °C
289 °F
ASTM D648
Kotec Carbotex KG-15MRA Polycarbonate, 15% Glass Fiber Reinforced
Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
Heat Distortion Temperature 143 °C
289 °F
ASTM D648
Kotec Carbotex KGN-15MRA Polycarbonate, Flame Retardant, 15% Glass Fiber Reinforced
Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
Heat Distortion Temperature 143 °C
289 °F
DIN 53 461, ISO R 75 process A
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al..