Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 54.4 °C | 130 °F | |
BCC Products BC 7062-2H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |