Polymer Property : Heat Distortion Temperature = 126 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 52.0 °C
126 °F
3M Scotchkote™ RG 501 Urethane Metal Repair
Scotchkote Urethane Metal Repair RG 501 has been specifically developed as a rapid curing repair system for rebuilding and repairing equipment requiring good mechanical strength.Product Features:Com..