Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 40.0 °C | 104 °F | HDT B; ISO 75 |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Heat Distortion Temperature | 40.0 °C | 104 °F | |
3M Scotchkote™ SG 527 Epoxy Metal Repair Scotchkote Epoxy Metal Repair SG 527 is a specially packaged rapid curing synthetic metal repair compound for on site repairs to metal components such as leaking pipes, tanks, ducts, and radiators.P.. |