CTE, linear, Transverse to Flow 176 µm/m-°C

@Temperature 23.0 - 150 °C
97.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.