CTE, linear, Transverse to Flow 91.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
50.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.