Polymer Property : CTE, linear, Transverse to Flow = 82.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 149 µm/m-°C

@Temperature 23.0 - 150 °C
82.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
CTE, linear, Transverse to Flow 149 µm/m-°C

@Temperature -40.0 - 40.0 °C
82.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal
LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
CTE, linear, Transverse to Flow 149 µm/m-°C

@Temperature -40.0 - 40.0 °C
82.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal
LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
CTE, linear, Transverse to Flow 149 µm/m-°C

@Temperature >=250 °C
82.8 µin/in-°F

@Temperature >=482 °F
z (> Tg); IPC TM-650 2.4.24
Arlon 85N Polyimide Laminate and Prepreg
85N is a polyimide and laminate prepreg system for PWBs requiring resistance to high temperature, both in process and in end-use application. Bromine-free chemistry provides thermal stability for a..