Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 79.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66 LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 79.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |