Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 76.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12 LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |