Polymer Property : CTE, linear, Transverse to Flow = 75.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 136 µm/m-°C

@Temperature 23.0 - 55.0 °C
75.6 µin/in-°F

@Temperature 73.4 - 131 °F
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
CTE, linear, Transverse to Flow 136 µm/m-°C

@Temperature 23.0 - 55.0 °C
75.6 µin/in-°F

@Temperature 73.4 - 131 °F
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin
Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..