Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 69.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
CTE, linear, Transverse to Flow | 69.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
CTE, linear, Transverse to Flow | 69.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
CTE, linear, Transverse to Flow | 69.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
CTE, linear, Transverse to Flow | 69.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
CTE, linear, Transverse to Flow | 69.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |