Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 121 µm/m-°C @Temperature 55.0 - 160 °C |
67.2 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 121 µm/m-°C @Temperature 55.0 - 160 °C |
67.2 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |