Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 66.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP
LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral.
CTE, linear, Transverse to Flow 66.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer
Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion ..
CTE, linear, Transverse to Flow 66.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer
Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion ..