Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 60.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 60.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |