Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 59.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP LNP THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled. |