Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 310 µm/m-°C @Temperature 55.0 - 120 °C |
172 µin/in-°F @Temperature 131 - 248 °F |
ASTM E 831 |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
CTE, linear, Transverse to Flow | 310 µm/m-°C @Temperature 55.0 - 120 °C |
172 µin/in-°F @Temperature 131 - 248 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |