Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 49.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
CTE, linear, Transverse to Flow | 49.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
CTE, linear, Transverse to Flow | 49.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 49.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |