Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 2.00 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 3.60 µm/m-°C

@Temperature -40.0 - 40.0 °C
2.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES
LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber.
CTE, linear, Transverse to Flow 3.60 µm/m-°C

@Temperature -40.0 - 40.0 °C
2.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES (Asia Pacific)
LNP* Thermocomp* JF003XXZ is a compound based on Polyethersulfone resin containing Glass Fiber.
CTE, linear, Transverse to Flow 3.60 µm/m-°C

@Temperature -40.0 - 40.0 °C
2.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 3.60 µm/m-°C

@Temperature -40.0 - 40.0 °C
2.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific)