Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 167 µm/m-°C @Temperature 55.0 - 100 °C |
92.8 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |