Polymer Property : CTE, linear, Transverse to Flow = 13.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Temperature 20.0 °C
13.3 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound which provides a good combination of mechanical and electrical properties.Applicati..
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU (Asia Pacific)
LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame..
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific)
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi..
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Thickness 4.00 mm,
Temperature 125 °C
13.3 µin/in-°F

@Thickness 0.157 in,
Temperature 257 °F
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Thickness 4.00 mm,
Temperature 25.0 °C
13.3 µin/in-°F

@Thickness 0.157 in,
Temperature 77.0 °F
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU
LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible.