Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature 23.0 - 150 °C
58.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East)
VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -30.0 - 80.0 °C
58.3 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQNH4550 PBT
Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% ..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -30.0 - 80.0 °C
58.3 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON MD000 PP
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific)
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific)
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific)
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East)
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific)
General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Europe-Africa-Middle East)
General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific)
Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific)
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER
PC+Polyester, UV Stabilized, Transparent
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER
PC+Polyester, UV Stabilized, Transparent
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific)
Transparent, US Food Contact compliant, chemically resistant. This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East)
Transparent, US Food Contact compliant, chemically resistant. This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester, UV Stabilized, Transparent
CTE, linear, Transverse to Flow 105 µm/m-°C

@Thickness 2.00 mm,
Temperature 160 - 260 °C
58.3 µin/in-°F

@Thickness 0.0787 in,
Temperature 320 - 500 °F
ISO 11359-1/-2
Celanese Zenite® ZE55801 NC010 LCP
Zenite® ZE55801 NC010 is a 30% glass reinforced, lubricated liquid crystal polymer resin designed for enhanced electroless plating.Celenese acquired the Zenite product line from DuPont in 2010.