Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS
LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific)
LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer
LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
CTE, linear, Parallel to Flow 96.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Copyright © lookpolymers.com All Rights Reserved