Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC (Asia Pacific)
LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Easy Molding, Flame Retardant.
CTE, linear, Parallel to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched
LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC
LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Flame Retardant.
CTE, linear, Parallel to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP
LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized.
CTE, linear, Parallel to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific)
LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa..