CTE, linear, Parallel to Flow 68.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP
LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized.