Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 117 µm/m-°C @Temperature 25.6 - 93.3 °C |
65.0 µin/in-°F @Temperature 78.0 - 200 °F |
Length |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |