Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DX04462C PC
LNP STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
CTE, linear, Parallel to Flow 63.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DX04490 PC
LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
CTE, linear, Parallel to Flow 63.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DX04462C PC (Asia Pacific)
LNP* STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System.
CTE, linear, Parallel to Flow 63.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific)
LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.