Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 57.3 µm/m-°C @Temperature 23.0 - 150 °C |
31.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East) 10% GF FR PBT/PC Blend |