Polymer Property : CTE, linear, Parallel to Flow = 5.61 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
5.61 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DEI13F PC
LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R..