Polymer Property : CTE, linear, Parallel to Flow = 43.5 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
CTE, linear, Parallel to Flow 43.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
CTE, linear, Parallel to Flow 43.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific)
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
CTE, linear, Parallel to Flow 43.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific)
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..