Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 72.3 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |